FGD Corrosion

State-of-the-art flue gas desulfurization (FGD) technologies continue to be installed on most large coal fired electric generating units in response to new regulatory emission requirements. Aggressive corrosion has been noted in some of these systems, presumably from the low pH, high chloride environments created in the FGD process.

Stress’ Creep Laboratory

Creep Laboratory for High Temperature Remaining Life Assessment:  Our facility includes 68 fully instrumented creep machines ranging in capacity from 3000 lbs up to 100,000 lbs.

Scoop Sampling

Stress Engineering Services (SES) performs material condition assessments on vessels and high temperature plants by extracting small material samples commonly referred to as “small scoop” samples. These samples can be taken at various depths so that minimum wall is not violated and weld repairs are not needed.